Chromium is the clearest case in water treatment where the oxidation state, not the element, decides the process. Trivalent chromium is a cation that precipitates as hydroxide at pH 8-9 and is captured by ordinary cation resin. Hexavalent chromium is an oxyanion, present as chromate, hydrogen chromate or dichromate depending on pH and concentration, and it passes through a cation bed untouched. Any treatment design that does not separate the two will fail on one of them, and the analytical method must report them separately.
The dominant industrial route is weak base anion exchange. Acrylic weak base resin, operating at pH 4-6, protonates its amine groups and exchanges chromate for hydroxide or chloride. Capacities of 1.1-1.4 eq/L are typical, and the practical loading is often limited by the sulfate and chloride in the stream rather than by the resin. Because the resin is weak base, it is regenerated with 4-8% sodium hydroxide at 2-4 bed volumes, which converts the amine back to the free base form and releases a sodium chromate solution concentrated enough to be reused in the plating bath or sent to a chrome recovery circuit.
Strong base anion resin also works and is more tolerant of low pH, but it is harder to regenerate and it will pick up sulfate preferentially in many mixed plating effluents. This matters in plants that rinse both chrome and nickel lines into a common collector: the sulfate from nickel sulfate plating and the chloride from acid copper will load the anion bed ahead of chromate and shorten the run length dramatically. Segregating the chrome rinse stream is almost always cheaper than upsizing the resin bed.
The alternative route uses a strong acid cation resin in the hydrogen form. At pH below 3, the resin donates protons and the chromate is reduced to trivalent chromium at the resin surface, and the resulting Cr(III) is then held by the cation resin itself. The advantage is that one bed handles both oxidation states and the eluate is a mixed chrome solution suitable for returning to a tanning or plating bath. The disadvantage is acid consumption: the bed must be regenerated with sulfuric or hydrochloric acid, and the effluent load shifts from chrome to acid.
Whichever route is chosen, the pretreatment is the same. Hexavalent chromium rinse water usually carries suspended hydroxide floc, oil and, in hard water areas, calcium that will precipitate as sulfate or carbonate inside the bed. Filtration to 10 microns and, where hardness exceeds 150 mg/L as calcium carbonate, a softening or acidification step keep the anion bed from cementing. Temperature is the other constraint: weak base acrylic resin loses capacity above about 60 degrees Celsius, and hot chrome rinse water is common enough that a cooling step is worth checking.
Eluate management decides whether the process is a cost or a credit. A well-run weak base system produces 1-2 bed volumes of eluate at 5-20 g/L chromium, which is a usable strength for bath make-up. Dilute eluate, below 2 g/L, is usually treated by reduction and precipitation, so the way regeneration is sequenced, with a slow caustic introduction and a hold, directly affects whether the plant has a product or a waste. Splitting the eluate, taking the first and richest fraction for reuse and sending the tail to treatment, is a simple practice that many plants overlook.
Finally, monitoring. Chromate breakthrough is sharp but not instantaneous, and the analytical method matters: diphenylcarbazide colorimetry reads Cr(VI) specifically and is the only suitable field method, while atomic absorption gives total chromium and will hide a failure. A bed that reports low total chromium while passing Cr(VI) is a real and common failure mode, and it is invisible without species-specific testing.